General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 7.15 g/cm³ Show Material materials with Density of 7.15 g/cm³ | Typical for Ductile (Nodular) Cast Iron |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 165 - 180 GPa Show Material materials with Elastic modulus of 165 - 180 GPa | Typical for Ductile (Nodular) Cast Iron |
Elongation | 20.0 °C | 2 % Show Material materials with Elongation of 2 % | |
Hardness, Brinell | 20.0 °C | 210 - 260 [-] Show Material materials with Hardness, Brinell of 210 - 260 [-] | |
Poisson's ratio | 23.0 °C | 0.26 - 0.31 [-] Show Material materials with Poisson's ratio of 0.26 - 0.31 [-] | Typical for Ductile (Nodular) Cast Iron |
Shear modulus | 23.0 °C | 63 - 66 GPa Show Material materials with Shear modulus of 63 - 66 GPa | Typical for Ductile (Nodular) Cast Iron |
Tensile strength | 20.0 °C | 650 MPa Show Material materials with Tensile strength of 650 MPa | |
Yield strength | 20.0 °C | 430 MPa Show Material materials with Yield strength of 430 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1E-5 - 1.6E-5 1/K Show Material materials with Coefficient of thermal expansion of 1E-5 - 1.6E-5 1/K | Typical for Ductile (Nodular) Cast Iron |
Melting point | 1150 - 1200 °C Show Material materials with Melting point of 1150 - 1200 °C | Typical for Ductile (Nodular) Cast Iron | |
Specific heat capacity | 23.0 °C | 460 - 502 J/(kg·K) Show Material materials with Specific heat capacity of 460 - 502 J/(kg·K) | Typical for Ductile (Nodular) Cast Iron |
Thermal conductivity | 23.0 °C | 13 - 42 W/(m·K) Show Material materials with Thermal conductivity of 13 - 42 W/(m·K) | Typical for Ductile (Nodular) Cast Iron |
Chemical properties
Property | Value |
---|---|
Carbon | 2.3 - 2.6 % Show Material materials with Carbon of 2.3 - 2.6 % |
Manganese | 0.4 - 0.5 % Show Material materials with Manganese of 0.4 - 0.5 % |
Silicon | 1.2 - 1.5 % Show Material materials with Silicon of 1.2 - 1.5 % |
Sulfur | 0.1 - 0.15 % Show Material materials with Sulfur of 0.1 - 0.15 % |