Material EN-GJMB-550-4 (former GTS-55-04 acc. to DIN 1692-82) is an all-black malleable cast iron which is used for crankshafts, camshafts, rocking levers, shift-forks, spring brackets, swivel heads, joint flanges, wheel hubs, rear-axle casings, water barriers, pivot bearings as well as for pinion cages for automatic transmissions.

Related Standards

This material data has been provided by WIAM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

20.0 °C

7.2 - 7.5 g/cm³

Show Material materials with Density of 7.2 - 7.5 g/cm³

Mechanical

PropertyTemperatureValueComment

Elastic modulus

20.0 °C

175 - 195 GPa

Show Material materials with Elastic modulus of 175 - 195 GPa

Hardness, Brinell

20.0 °C

180 - 230 [-]

Show Material materials with Hardness, Brinell of 180 - 230 [-]

Poisson's ratio

23.0 °C

0.27 [-]

Show Material materials with Poisson's ratio of 0.27 [-]

Typical for Cast Iron

Shear modulus

23.0 °C

41 GPa

Show Material materials with Shear modulus of 41 GPa

Typical for Cast Iron

Tensile strength

20.0 °C

550 MPa

Show Material materials with Tensile strength of 550 MPa

Yield strength Rp0.2

20.0 °C

340 MPa

Show Material materials with Yield strength Rp0.2 of 340 MPa

Thermal

PropertyTemperatureValueComment

Melting point

1120 °C

Show Material materials with Melting point of 1120 °C

Typical for Cast Iron

Specific heat capacity

20.0 °C

460 - 500 J/(kg·K)

Show Material materials with Specific heat capacity of 460 - 500 J/(kg·K)

Thermal conductivity

20.0 °C

50 - 63 W/(m·K)

Show Material materials with Thermal conductivity of 50 - 63 W/(m·K)

Electrical

PropertyTemperatureValue

Electrical resistivity

20.0 °C

3E-7 - 4E-7 Ω·m

Show Material materials with Electrical resistivity of 3E-7 - 4E-7 Ω·m

Chemical properties

PropertyValue

Carbon

2.3 - 2.6 %

Show Material materials with Carbon of 2.3 - 2.6 %

Manganese

0.4 - 0.5 %

Show Material materials with Manganese of 0.4 - 0.5 %

Silicon

1.2 - 1.5 %

Show Material materials with Silicon of 1.2 - 1.5 %

Sulfur

0.1 - 0.15 %

Show Material materials with Sulfur of 0.1 - 0.15 %