JIS G4902 Grade NCF80A ageing treatment after solution treatment

Want to keep this datasheet? Save it now in your required format

Related Standards

Equivalent Materials

This material data has been provided by Japanese Industrial Standards.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Mechanical

PropertyTemperatureValue

Elongation A5

20.0 °C

15 - 25 %

Show Material materials with Elongation A5 of 15 - 25 %

Hardness, Brinell

20.0 °C

241 - 269 [-]

Show Material materials with Hardness, Brinell of 241 - 269 [-]

Hardness, Rockwell B

20.0 °C

100 [-]

Show Material materials with Hardness, Rockwell B of 100 [-]

Hardness, Rockwell C

20.0 °C

27 [-]

Show Material materials with Hardness, Rockwell C of 27 [-]

Hardness, Vickers

20.0 °C

250 - 285 [-]

Show Material materials with Hardness, Vickers of 250 - 285 [-]

Tensile strength

20.0 °C

1000 - 1030 MPa

Show Material materials with Tensile strength of 1000 - 1030 MPa

Yield strength Rp0.2

20.0 °C

615 - 635 MPa

Show Material materials with Yield strength Rp0.2 of 615 - 635 MPa

Chemical properties

PropertyValue

Aluminium

1 - 1.8 %

Show Material materials with Aluminium of 1 - 1.8 %

Carbon

0.04 - 0.1 %

Show Material materials with Carbon of 0.04 - 0.1 %

Chromium

18 - 21 %

Show Material materials with Chromium of 18 - 21 %

Copper

0.2 %

Show Material materials with Copper of 0.2 %

Iron

1.5 %

Show Material materials with Iron of 1.5 %

Manganese

1 %

Show Material materials with Manganese of 1 %

Phosphorus

0.03 %

Show Material materials with Phosphorus of 0.03 %

Silicon

1 %

Show Material materials with Silicon of 1 %

Sulfur

0.015 %

Show Material materials with Sulfur of 0.015 %

Titanium

1.8 - 2.7 %

Show Material materials with Titanium of 1.8 - 2.7 %

Technological properties

Property
Processing history

ageing treatment after solution treatment