Properties

Mechanical

PropertyTemperatureValue

Hardness, Rockwell B

23.0 °C

45 - 90 [-]

Show Material materials with Hardness, Rockwell B of 45 - 90 [-]

Hardness, Vickers

23.0 °C

85 - 195 [-]