Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

190 - 210 GPa

Show Material materials with Elastic modulus of 190 - 210 GPa

Typical for Soft Magnetic Iron

Hardness, Rockwell B

23.0 °C

45 - 90 [-]

Show Material materials with Hardness, Rockwell B of 45 - 90 [-]

Hardness, Vickers

23.0 °C

85 - 195 [-]

Show Material materials with Hardness, Vickers of 85 - 195 [-]

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

2E-6 - 1.2E-5 1/K

Show Material materials with Coefficient of thermal expansion of 2E-6 - 1.2E-5 1/K

Typical for Soft Magnetic Iron

Specific heat capacity

23.0 °C

470 J/(kg·K)

Show Material materials with Specific heat capacity of 470 J/(kg·K)

Typical for Soft Magnetic Iron

Thermal conductivity

23.0 °C

13 - 55 W/(m·K)

Show Material materials with Thermal conductivity of 13 - 55 W/(m·K)