Mechanical
Property | Temperature | Value |
---|---|---|
Elongation A50 | 20.0 °C | 40 % Show Material materials with Elongation A50 of 40 % |
Reduction of area | 20.0 °C | 50 % Show Material materials with Reduction of area of 50 % |
Tensile strength | 20.0 °C | 500 MPa Show Material materials with Tensile strength of 500 MPa |
Yield Strength Rp0.2, short transverse | 20.0 °C | 214 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 214 MPa |
Chemical properties
Property | Value |
---|---|
Carbon | 0.02 % Show Material materials with Carbon of 0.02 % |
Chromium | 26 - 28 % Show Material materials with Chromium of 26 - 28 % |
Copper | 0.6 - 1.4 % Show Material materials with Copper of 0.6 - 1.4 % |
Manganese | 2 % Show Material materials with Manganese of 2 % |
Molybdenum | 4 - 5 % Show Material materials with Molybdenum of 4 - 5 % |
Nickel | 30 - 34 % Show Material materials with Nickel of 30 - 34 % |
Phosphorus | 0.03 % Show Material materials with Phosphorus of 0.03 % |
Silicon | 0.6 % Show Material materials with Silicon of 0.6 % |
Sulfur | 0.015 % Show Material materials with Sulfur of 0.015 % |