Mechanical
Property | Temperature | Value |
---|---|---|
Elongation A50 | 20.0 °C | 2 % Show Material materials with Elongation A50 of 2 % |
Hardness, Rockwell Superficial 15-N | 20.0 °C | 78 [-] Show Material materials with Hardness, Rockwell Superficial 15-N of 78 [-] |
Hardness, Vickers | 20.0 °C | 320 [-] Show Material materials with Hardness, Vickers of 320 [-] |
Chemical properties
Property | Value |
---|---|
Carbon | 0.05 % Show Material materials with Carbon of 0.05 % |
Chromium | 2 - 3 % Show Material materials with Chromium of 2 - 3 % |
Cobalt | 0.5 % Show Material materials with Cobalt of 0.5 % |
Copper | 4 - 6 % Show Material materials with Copper of 4 - 6 % |
Manganese | 1.5 % Show Material materials with Manganese of 1.5 % |
Molybdenum | 0.5 % Show Material materials with Molybdenum of 0.5 % |
Nickel | 75 - 78 % Show Material materials with Nickel of 75 - 78 % |
Phosphorus | 0.02 % Show Material materials with Phosphorus of 0.02 % |
Silicon | 0.5 % Show Material materials with Silicon of 0.5 % |
Sulfur | 0.01 % Show Material materials with Sulfur of 0.01 % |