ASTM A297 Grade HW As-Cast

Want to keep this datasheet? Save it now in your required format

Related Standards

Equivalent Materials

This material data has been provided by ASTM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Mechanical

PropertyTemperatureValue

Tensile strength

20.0 °C

415 MPa

Show Material materials with Tensile strength of 415 MPa

Chemical properties

PropertyValue

Carbon

0.35 - 0.75 %

Show Material materials with Carbon of 0.35 - 0.75 %

Chromium

10 - 14 %

Show Material materials with Chromium of 10 - 14 %

Manganese

2 %

Show Material materials with Manganese of 2 %

Molybdenum

0.5 %

Show Material materials with Molybdenum of 0.5 %

Nickel

58 - 62 %

Show Material materials with Nickel of 58 - 62 %

Phosphorus

0.04 %

Show Material materials with Phosphorus of 0.04 %

Silicon

2.5 %

Show Material materials with Silicon of 2.5 %

Sulfur

0.04 %

Show Material materials with Sulfur of 0.04 %