ASTM A436 Grade Type 1

Want to keep this datasheet? Save it now in your required format

Related Standards

This material data has been provided by ASTM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Mechanical

PropertyTemperatureValue

Hardness, Brinell

23.0 °C

131 - 183 [-]

Show Material materials with Hardness, Brinell of 131 - 183 [-]

Tensile strength

23.0 °C

172 MPa

Show Material materials with Tensile strength of 172 MPa

Chemical properties

PropertyValue

Carbon

3 %

Show Material materials with Carbon of 3 %

Chromium

1.5 - 2.5 %

Show Material materials with Chromium of 1.5 - 2.5 %

Copper

5.5 - 7.5 %

Show Material materials with Copper of 5.5 - 7.5 %

Manganese

0.5 - 1.5 %

Show Material materials with Manganese of 0.5 - 1.5 %

Nickel

13.5 - 17.5 %

Show Material materials with Nickel of 13.5 - 17.5 %

Silicon

1 - 2.8 %

Show Material materials with Silicon of 1 - 2.8 %

Sulfur

0.12 %

Show Material materials with Sulfur of 0.12 %