Properties

Mechanical

PropertyTemperatureValue

Elongation A50

20.0 °C

10 %

Show Material materials with Elongation A50 of 10 %

Hardness, Brinell

20.0 °C

131 - 193 [-]

Show Material materials with Hardness, Brinell of 131 - 193 [-]

Tensile strength

20.0 °C

380 MPa

Show Material materials with Tensile strength of 380 MPa

Yield Strength Rp0.2, short transverse

20.0 °C

210 MPa

Show Material materials with Yield Strength Rp0.2, short transverse of 210 MPa

Chemical properties

PropertyValue

Carbon

2.3 %

Show Material materials with Carbon of 2.3 %

Chromium

1.75 - 2.25 %

Show Material materials with Chromium of 1.75 - 2.25 %

Manganese

1 %

Show Material materials with Manganese of 1 %

Nickel

34 - 37 %

Show Material materials with Nickel of 34 - 37 %

Phosphorus

0.08 %

Show Material materials with Phosphorus of 0.08 %

Silicon

4.9 - 5.5 %

Show Material materials with Silicon of 4.9 - 5.5 %