ASTM A447 25-12 Class Type I

Want to keep this datasheet? Save it now in your required format

Related Standards

This material data has been provided by ASTM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Mechanical

PropertyTemperatureValue

Elongation

23.0 °C

8.7 %

Show Material materials with Elongation of 8.7 %

Elongation A50

23.0 °C

9 %

Show Material materials with Elongation A50 of 9 %

Tensile strength

23.0 °C

550 MPa

Show Material materials with Tensile strength of 550 MPa

Chemical properties

PropertyValue

Carbon

0.2 - 0.45 %

Show Material materials with Carbon of 0.2 - 0.45 %

Chromium

23 - 28 %

Show Material materials with Chromium of 23 - 28 %

Manganese

2.5 %

Show Material materials with Manganese of 2.5 %

Nickel

10 - 14 %

Show Material materials with Nickel of 10 - 14 %

Nitrogen

0.2 %

Show Material materials with Nitrogen of 0.2 %

Phosphorus

0.03 %

Show Material materials with Phosphorus of 0.03 %

Silicon

1.75 %

Show Material materials with Silicon of 1.75 %

Sulfur

0.03 %

Show Material materials with Sulfur of 0.03 %