OUR COOKIE DISCLAIMER
Matmatch uses cookies and similar technologies to improve your experience and measure your interactions with our website. We also use them to provide you more relevant information and improve our platform and search tools. If that’s okay, click “Accept all.” To change your preferences, click “Open cookie settings.” You will find more information about cookies on our privacy policy page.
Open cookie settings
This material data has been provided by ASTM.
All categories
We can help
you to find a supplier
We will evaluate your request for ASTM A532 Class II Type A As Cast or As Cast and Stress Relieved and get back to you soon.
Do you supply similar materials?
List your company on Matmatch now and reach engineers around the world looking for such materials.
Mechanical
Property | Value | Temperature |
---|---|---|
Hardness, Brinell | 550 [-] Show Material materials with Hardness, Brinell of 550 [-] at 23.0 °C | 23.0 °C |
Hardness, Rockwell C | 53 [-] Show Material materials with Hardness, Rockwell C of 53 [-] at 23.0 °C | 23.0 °C |
Hardness, Vickers | 600 [-] Show Material materials with Hardness, Vickers of 600 [-] at 23.0 °C | 23.0 °C |
Chemical properties
Property | ||
---|---|---|
Carbon | 2 - 3.3 % | |
Chromium | 11 - 14 % | |
Copper | 1.2 % | |
Manganese | 2 % | |
Molybdenum | 3 % | |
Nickel | 2.5 % | |
Phosphorus | 0.1 % | |
Silicon | 1.5 % | |
Sulfur | 0.06 % |
MATMATCH
We connect engineers, product designers and procurement teams with the best materials and suppliers for their job.
COMPANY
CONTACT US
+49 89 262075200
Leopoldstraße 250 A, 80807 Munich
© 2021 Matmatch GmbH, All rights reserved.
Made with ♥ in Munich!