ASTM A532 Class II Type A

Want to keep this datasheet? Save it now in your required format

Related Standards

This material data has been provided by ASTM.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Mechanical

PropertyTemperatureValue

Hardness, Brinell

23.0 °C

550 [-]

Show Material materials with Hardness, Brinell of 550 [-]

Hardness, Rockwell C

23.0 °C

53 [-]

Show Material materials with Hardness, Rockwell C of 53 [-]

Hardness, Vickers

23.0 °C

600 [-]

Show Material materials with Hardness, Vickers of 600 [-]

Chemical properties

PropertyValue

Carbon

2 - 3.3 %

Show Material materials with Carbon of 2 - 3.3 %

Chromium

11 - 14 %

Show Material materials with Chromium of 11 - 14 %

Copper

1.2 %

Show Material materials with Copper of 1.2 %

Manganese

2 %

Show Material materials with Manganese of 2 %

Molybdenum

3 %

Show Material materials with Molybdenum of 3 %

Nickel

2.5 %

Show Material materials with Nickel of 2.5 %

Phosphorus

0.1 %

Show Material materials with Phosphorus of 0.1 %

Silicon

1.5 %

Show Material materials with Silicon of 1.5 %

Sulfur

0.06 %