ASTM A453 Grade 665 Class A

Want to keep this datasheet? Save it now in your required format

Related Standards

This material data has been provided by ASTM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Mechanical

PropertyTemperatureValue

Elongation A50

23.0 °C

12 %

Show Material materials with Elongation A50 of 12 %

Hardness, Brinell

23.0 °C

311 - 388 [-]

Show Material materials with Hardness, Brinell of 311 - 388 [-]

Hardness, Rockwell C

23.0 °C

32 - 41 [-]

Show Material materials with Hardness, Rockwell C of 32 - 41 [-]

Reduction of area

23.0 °C

15 %

Show Material materials with Reduction of area of 15 %

Tensile strength

23.0 °C

1170 MPa

Show Material materials with Tensile strength of 1170 MPa

Yield strength Rp0.2

23.0 °C

830 MPa

Show Material materials with Yield strength Rp0.2 of 830 MPa

Chemical properties

PropertyValue

Aluminium

0.25 %

Show Material materials with Aluminium of 0.25 %

Boron

0.01 - 0.07 %

Show Material materials with Boron of 0.01 - 0.07 %

Carbon

0.08 %

Show Material materials with Carbon of 0.08 %

Chromium

12 - 15 %

Show Material materials with Chromium of 12 - 15 %

Copper

0.25 %

Show Material materials with Copper of 0.25 %

Manganese

1.25 - 2 %

Show Material materials with Manganese of 1.25 - 2 %

Molybdenum

1.25 - 2.25 %

Show Material materials with Molybdenum of 1.25 - 2.25 %

Nickel

24 - 28 %

Show Material materials with Nickel of 24 - 28 %

Phosphorus

0.04 %

Show Material materials with Phosphorus of 0.04 %

Silicon

0.1 - 0.8 %

Show Material materials with Silicon of 0.1 - 0.8 %

Sulfur

0.03 %

Show Material materials with Sulfur of 0.03 %

Titanium

2.7 - 3.3 %

Show Material materials with Titanium of 2.7 - 3.3 %