Mechanical
Property | Temperature | Value |
---|---|---|
Elongation A50 | 23.0 °C | 15 % Show Material materials with Elongation A50 of 15 % |
Hardness, Brinell | 23.0 °C | 248 [-] Show Material materials with Hardness, Brinell of 248 [-] |
Reduction of area | 23.0 °C | 18 % Show Material materials with Reduction of area of 18 % |
Tensile strength | 23.0 °C | 895 MPa Show Material materials with Tensile strength of 895 MPa |
Yield strength Rp0.2 | 23.0 °C | 585 MPa Show Material materials with Yield strength Rp0.2 of 585 MPa |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.35 % Show Material materials with Aluminium of 0.35 % |
Boron | 0.001 - 0.01 % Show Material materials with Boron of 0.001 - 0.01 % |
Carbon | 0.08 % Show Material materials with Carbon of 0.08 % |
Chromium | 13.5 - 16 % Show Material materials with Chromium of 13.5 - 16 % |
Manganese | 2 % Show Material materials with Manganese of 2 % |
Molybdenum | 1 - 1.5 % Show Material materials with Molybdenum of 1 - 1.5 % |
Nickel | 24 - 27 % Show Material materials with Nickel of 24 - 27 % |
Phosphorus | 0.04 % Show Material materials with Phosphorus of 0.04 % |
Silicon | 1 % Show Material materials with Silicon of 1 % |
Sulfur | 0.03 % Show Material materials with Sulfur of 0.03 % |
Titanium | 1.9 - 2.35 % Show Material materials with Titanium of 1.9 - 2.35 % |
Vanadium | 0.1 - 0.5 % Show Material materials with Vanadium of 0.1 - 0.5 % |