Matmatch uses cookies and similar technologies to improve your experience and measure your interactions with our website. We also use them to provide you more relevant information and improve our platform and search tools. If that’s okay, click “Accept all.” To change your preferences, click “Open cookie settings.” You will find more information about cookies on our privacy policy page.
Open cookie settings
Find Materials
Categories
This material data has been provided by ASTM.
All categories
Let us help you find the best supplier!
List your company on Matmatch now and reach engineers around the world looking for such materials.
Request more informationMechanical
Property | Temperature | Value |
---|---|---|
Elongation A50 | 23.0 °C | 7 % Show Material materials with Elongation A50 of 7 % |
Hardness, Brinell | 23.0 °C | 302 - 375 [-] Show Material materials with Hardness, Brinell of 302 - 375 [-] |
Tensile strength | 23.0 °C | 1050 MPa Show Material materials with Tensile strength of 1050 MPa |
Yield strength Rp0.2 | 23.0 °C | 750 MPa Show Material materials with Yield strength Rp0.2 of 750 MPa |
MATMATCH
We connect engineers, product designers and procurement teams with the best materials and suppliers for their job.
COMPANY
CONTACT US
Siebenbürger Str. 23, 86983 Lechbruck am See, Germany
© 2024 Plansee Composite Materials GmbH, All rights reserved.