ASTM A240 Grade N08020 Heat-Treated

Want to keep this datasheet? Save it now in your required format

Related Standards

Equivalent Materials

This material data has been provided by ASTM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Mechanical

PropertyTemperatureValue

Elongation A50

20.0 °C

30 %

Show Material materials with Elongation A50 of 30 %

Hardness, Brinell

20.0 °C

217 [-]

Show Material materials with Hardness, Brinell of 217 [-]

Hardness, Rockwell B

20.0 °C

95 [-]

Show Material materials with Hardness, Rockwell B of 95 [-]

Tensile strength

20.0 °C

550 MPa

Show Material materials with Tensile strength of 550 MPa

Yield Strength Rp0.2, short transverse

20.0 °C

240 MPa

Show Material materials with Yield Strength Rp0.2, short transverse of 240 MPa

Chemical properties

PropertyValue

Carbon

0.07 %

Show Material materials with Carbon of 0.07 %

Chromium

19 - 21 %

Show Material materials with Chromium of 19 - 21 %

Copper

3 - 4 %

Show Material materials with Copper of 3 - 4 %

Manganese

2 %

Show Material materials with Manganese of 2 %

Molybdenum

2 - 3 %

Show Material materials with Molybdenum of 2 - 3 %

Nickel

32 - 38 %

Show Material materials with Nickel of 32 - 38 %

Phosphorus

0.05 %

Show Material materials with Phosphorus of 0.05 %

Silicon

1 %

Show Material materials with Silicon of 1 %

Sulfur

0.035 %

Show Material materials with Sulfur of 0.035 %