General
Property | Value | Comment |
---|---|---|
Density | 4.506 g/cm³ Show Material materials with Density of 4.506 g/cm³ | Typical for Pure Titanium |
Mechanical
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Elastic modulus | 120.0 GPa Show Material materials with Elastic modulus of 120.0 GPa | Typical for Pure Titanium | |||
Elongation | 23.0 % Show Material materials with Elongation of 23.0 % | Welded | JIS H4630 | Tube, Pipe | |
Poisson's ratio | 0.361 [-] Show Material materials with Poisson's ratio of 0.361 [-] | Typical for Pure Titanium | |||
Shear modulus | 46.0 GPa Show Material materials with Shear modulus of 46.0 GPa | Typical for Pure Titanium | |||
Tensile strength | 343.0 MPa Show Material materials with Tensile strength of 343.0 MPa | Welded | JIS H4630 | Tube, Pipe |
Thermal
Property | Value | Comment |
---|---|---|
Coefficient of thermal expansion | 8.400000000000001e-06 - 8.599999999999999e-06 1/K Show Material materials with Coefficient of thermal expansion of 8.400000000000001e-06 - 8.599999999999999e-06 1/K | Typical for Pure Titanium |
Melting point | 1670.0 °C Show Material materials with Melting point of 1670.0 °C | Typical for Pure Titanium |
Specific heat capacity | 513.0 - 599.0 J/(kg·K) Show Material materials with Specific heat capacity of 513.0 - 599.0 J/(kg·K) | Typical for Pure Titanium |
Thermal conductivity | 15.0 - 22.0 W/(m·K) Show Material materials with Thermal conductivity of 15.0 - 22.0 W/(m·K) | Typical for Pure Titanium |
Technological properties
Property | ||
---|---|---|
Processing history | welded |