Mechanical
Chemical properties
Property | Value |
---|---|
Carbon | 0.35 % Show Material materials with Carbon of 0.35 % |
Copper | 26 - 33 % Show Material materials with Copper of 26 - 33 % |
Iron | 3.5 % Show Material materials with Iron of 3.5 % |
Manganese | 1.5 % Show Material materials with Manganese of 1.5 % |
Niobium | 0.5 % Show Material materials with Niobium of 0.5 % |
Phosphorus | 0.03 % Show Material materials with Phosphorus of 0.03 % |
Silicon | 2 % Show Material materials with Silicon of 2 % |
Sulfur | 0.02 % Show Material materials with Sulfur of 0.02 % |