Property | Value |
---|---|
Carbon | 0.02 % Show Material materials with Carbon of 0.02 % |
Chromium | 15 - 17.5 % Show Material materials with Chromium of 15 - 17.5 % |
Iron | 2 % Show Material materials with Iron of 2 % |
Manganese | 1 % Show Material materials with Manganese of 1 % |
Molybdenum | 15 - 17.5 % Show Material materials with Molybdenum of 15 - 17.5 % |
Phosphorus | 0.03 % Show Material materials with Phosphorus of 0.03 % |
Silicon | 0.8 % Show Material materials with Silicon of 0.8 % |
Sulfur | 0.015 % Show Material materials with Sulfur of 0.015 % |
Tungsten | 1 % Show Material materials with Tungsten of 1 % |