Mechanical
Chemical properties
Property | Value |
---|---|
Carbon | 0.03 % Show Material materials with Carbon of 0.03 % |
Chromium | 19 - 22 % Show Material materials with Chromium of 19 - 22 % |
Copper | 3 - 3.5 % Show Material materials with Copper of 3 - 3.5 % |
Manganese | 1.5 % Show Material materials with Manganese of 1.5 % |
Molybdenum | 2 - 3 % Show Material materials with Molybdenum of 2 - 3 % |
Nickel | 27.5 - 30.5 % Show Material materials with Nickel of 27.5 - 30.5 % |
Phosphorus | 0.03 % Show Material materials with Phosphorus of 0.03 % |
Silicon | 1 % Show Material materials with Silicon of 1 % |
Sulfur | 0.015 % Show Material materials with Sulfur of 0.015 % |