General
Property | Value | Temperature |
---|---|---|
Density | 9 g/cm³ Show Material materials with Density of 9 g/cm³ at 23.0 °C | 23.0 °C |
Mechanical
Property | Value | Temperature |
---|---|---|
Elastic modulus | 160 GPa Show Material materials with Elastic modulus of 160 GPa at 23.0 °C | 23.0 °C |
Elongation | 29 % Show Material materials with Elongation of 29 % at 23.0 °C | 23.0 °C |
Tensile strength | 550 MPa Show Material materials with Tensile strength of 550 MPa at 23.0 °C | 23.0 °C |
Yield strength | 240 MPa Show Material materials with Yield strength of 240 MPa at 23.0 °C | 23.0 °C |
Thermal
Property | Value | Temperature | Comment |
---|---|---|---|
Coefficient of thermal expansion | 1.5E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.5E-5 1/K at 23.0 °C | 23.0 °C | |
Melting point | 1170 - 1365 °C Show Material materials with Melting point of 1170 - 1365 °C | Typical for Nickel Copper Alloy | |
Specific heat capacity | 430 J/(kg·K) Show Material materials with Specific heat capacity of 430 J/(kg·K) at 23.0 °C | 23.0 °C | |
Thermal conductivity | 16 - 45 W/(m·K) Show Material materials with Thermal conductivity of 16 - 45 W/(m·K) at 23.0 °C | 23.0 °C | Typical for Nickel Copper Alloy |
Chemical properties
Property | ||
---|---|---|
Carbon | 0 - 0.3 % | |
Copper | 28 - 34 % | |
Iron | 0 - 2.5 % | |
Manganese | 0 - 2 % | |
Nickel | 63 - 72 % | |
Silicon | 0 - 0.5 % | |
Sulfur | 0.025 - 0.06 % |