ASTM Grade 19 Moderate Strength

Want to keep this datasheet? Save it now in your required format

Equivalent Materials

This material data has been provided by MakeItFrom.com.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueTemperature

Density

5 g/cm³

Show Material materials with Density of 5 g/cm³ at 23.0 °C

23.0 °C

Mechanical

PropertyValueTemperature

Elastic modulus

100 GPa

Show Material materials with Elastic modulus of 100 GPa at 23.0 °C

23.0 °C

Elongation

12 %

Show Material materials with Elongation of 12 % at 23.0 °C

23.0 °C

Tensile strength

1070 MPa

Show Material materials with Tensile strength of 1070 MPa at 23.0 °C

23.0 °C

Yield strength

980 MPa

Show Material materials with Yield strength of 980 MPa at 23.0 °C

23.0 °C

Thermal

PropertyValueTemperatureComment

Coefficient of thermal expansion

9.5E-6 1/K

Show Material materials with Coefficient of thermal expansion of 9.5E-6 1/K at 23.0 °C

23.0 °C

Melting point

1550 - 1815 °C

Show Material materials with Melting point of 1550 - 1815 °C

Typical for Titanium Beta Alloy

Specific heat capacity

520 J/(kg·K)

Show Material materials with Specific heat capacity of 520 J/(kg·K) at 23.0 °C

23.0 °C

Thermal conductivity

6.2 W/(m·K)

Show Material materials with Thermal conductivity of 6.2 W/(m·K) at 23.0 °C

23.0 °C

Chemical properties

Property

Aluminium

3 - 4 %

Carbon

0 - 0.05 %

Chromium

5.5 - 6.5 %

Hydrogen

0 - 0.02 %

Iron

0 - 0.3 %

Molybdenum

3.5 - 4.5 %

Nitrogen

0 - 0.03 %

Other

0 - 0.4 %

Oxygen

0 - 0.12 %

Titanium

71.1 - 77 %

Vanadium

7.5 - 8.5 %

Zirconium

3.5 - 4.5 %