General
Property | Value | Temperature |
---|---|---|
Density | 5 g/cm³ Show Material materials with Density of 5 g/cm³ at 23.0 °C | 23.0 °C |
Mechanical
Property | Value | Temperature |
---|---|---|
Elastic modulus | 130 GPa Show Material materials with Elastic modulus of 130 GPa at 23.0 °C | 23.0 °C |
Elongation | 12 % Show Material materials with Elongation of 12 % at 23.0 °C | 23.0 °C |
Tensile strength | 1070 MPa Show Material materials with Tensile strength of 1070 MPa at 23.0 °C | 23.0 °C |
Yield strength | 980 MPa Show Material materials with Yield strength of 980 MPa at 23.0 °C | 23.0 °C |
Thermal
Property | Value | Temperature | Comment |
---|---|---|---|
Coefficient of thermal expansion | 9.6E-6 1/K Show Material materials with Coefficient of thermal expansion of 9.6E-6 1/K at 23.0 °C | 23.0 °C | |
Melting point | 1550 - 1815 °C Show Material materials with Melting point of 1550 - 1815 °C | Typical for Titanium Beta Alloy | |
Specific heat capacity | 510 J/(kg·K) Show Material materials with Specific heat capacity of 510 J/(kg·K) at 23.0 °C | 23.0 °C | |
Thermal conductivity | 6 - 11 W/(m·K) Show Material materials with Thermal conductivity of 6 - 11 W/(m·K) at 23.0 °C | 23.0 °C | Typical for Titanium Beta Alloy |
Chemical properties
Property | ||
---|---|---|
Aluminium | 3 - 4 % | |
Carbon | 0 - 0.05 % | |
Chromium | 5.5 - 6.5 % | |
Hydrogen | 0 - 0.02 % | |
Iron | 0 - 0.3 % | |
Molybdenum | 3.5 - 4.5 % | |
Nitrogen | 0 - 0.03 % | |
Other | 0 - 0.4 % | |
Oxygen | 0 - 0.12 % | |
Palladium | 0.04 - 0.08 % | |
Titanium | 71 - 77 % | |
Vanadium | 7.5 - 8.5 % | |
Zirconium | 3.5 - 4.5 % |