ZA-12 Permanent Mold

Want to keep this datasheet? Save it now in your required format

This material data has been provided by MakeItFrom.com.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

20.0 °C

6 g/cm³

Show Material materials with Density of 6 g/cm³

Mechanical

PropertyTemperatureValue

Elastic modulus

20.0 °C

83 GPa

Show Material materials with Elastic modulus of 83 GPa

Elongation

20.0 °C

1.9 %

Show Material materials with Elongation of 1.9 %

Tensile strength

20.0 °C

290 MPa

Show Material materials with Tensile strength of 290 MPa

Yield strength

20.0 °C

270 MPa

Show Material materials with Yield strength of 270 MPa

Thermal

PropertyTemperatureValue

Coefficient of thermal expansion

20.0 °C

2.4E-5 1/K

Show Material materials with Coefficient of thermal expansion of 2.4E-5 1/K

Melting point

380 °C

Show Material materials with Melting point of 380 °C

Specific heat capacity

20.0 °C

450 J/(kg·K)

Show Material materials with Specific heat capacity of 450 J/(kg·K)

Thermal conductivity

20.0 °C

120 W/(m·K)

Show Material materials with Thermal conductivity of 120 W/(m·K)

Chemical properties

PropertyValue

Aluminium

10.5 - 11.5 %

Show Material materials with Aluminium of 10.5 - 11.5 %

Cadmium

6E-3 %

Show Material materials with Cadmium of 6E-3 %

Copper

0.5 - 1.2 %

Show Material materials with Copper of 0.5 - 1.2 %

Iron

0.08 %

Show Material materials with Iron of 0.08 %

Lead

6E-3 %

Show Material materials with Lead of 6E-3 %

Magnesium

0.02 - 0.03 %

Show Material materials with Magnesium of 0.02 - 0.03 %

Nickel

0.02 %

Show Material materials with Nickel of 0.02 %

Silicon

0.06 %

Show Material materials with Silicon of 0.06 %

Tin

3E-3 %

Show Material materials with Tin of 3E-3 %

Zinc

87.1 - 89 %

Show Material materials with Zinc of 87.1 - 89 %