ZA-27 Sand Cast

Want to keep this datasheet? Save it now in your required format

This material data has been provided by MakeItFrom.com.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

5 g/cm³

Show Material materials with Density of 5 g/cm³

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

78 GPa

Show Material materials with Elastic modulus of 78 GPa

Elongation

23.0 °C

4.5 %

Show Material materials with Elongation of 4.5 %

Poisson's ratio

23.0 °C

0.3 [-]

Show Material materials with Poisson's ratio of 0.3 [-]

Typical for Zinc Aluminium

Tensile strength

23.0 °C

420 MPa

Show Material materials with Tensile strength of 420 MPa

Yield strength

23.0 °C

370 MPa

Show Material materials with Yield strength of 370 MPa

Thermal

PropertyTemperatureValue

Coefficient of thermal expansion

23.0 °C

2.6E-5 1/K

Show Material materials with Coefficient of thermal expansion of 2.6E-5 1/K

Melting point

380 °C

Show Material materials with Melting point of 380 °C

Specific heat capacity

23.0 °C

530 J/(kg·K)

Show Material materials with Specific heat capacity of 530 J/(kg·K)

Thermal conductivity

23.0 °C

130 W/(m·K)

Show Material materials with Thermal conductivity of 130 W/(m·K)

Chemical properties

PropertyValue

Aluminium

25 - 28 %

Show Material materials with Aluminium of 25 - 28 %

Cadmium

0 - 6E-3 %

Show Material materials with Cadmium of 0 - 6E-3 %

Copper

2 - 2.5 %

Show Material materials with Copper of 2 - 2.5 %

Iron

0 - 0.1 %

Show Material materials with Iron of 0 - 0.1 %

Lead

0 - 6E-3 %

Show Material materials with Lead of 0 - 6E-3 %

Magnesium

0.01 - 0.02 %

Show Material materials with Magnesium of 0.01 - 0.02 %

Nickel

0 - 0.02 %

Show Material materials with Nickel of 0 - 0.02 %

Silicon

0 - 0.08 %

Show Material materials with Silicon of 0 - 0.08 %

Tin

0 - 3E-3 %

Show Material materials with Tin of 0 - 3E-3 %

Zinc

69.3 - 73 %