General
Property | Temperature | Value |
---|---|---|
Density | 23.0 °C | 4.4 g/cm³ Show Material materials with Density of 4.4 g/cm³ |
Mechanical
Property | Temperature | Value |
---|---|---|
Elastic modulus | 23.0 °C | 120 GPa Show Material materials with Elastic modulus of 120 GPa |
Elongation | 23.0 °C | 8.7 % Show Material materials with Elongation of 8.7 % |
Tensile strength | 23.0 °C | 1200 MPa Show Material materials with Tensile strength of 1200 MPa |
Yield strength | 23.0 °C | 1130 MPa Show Material materials with Yield strength of 1130 MPa |
Thermal
Property | Temperature | Value |
---|---|---|
Coefficient of thermal expansion | 23.0 °C | 8.9E-6 1/K Show Material materials with Coefficient of thermal expansion of 8.9E-6 1/K |
Melting point | 1650 °C Show Material materials with Melting point of 1650 °C | |
Specific heat capacity | 23.0 °C | 560 J/(kg·K) Show Material materials with Specific heat capacity of 560 J/(kg·K) |
Thermal conductivity | 23.0 °C | 6.8 W/(m·K) Show Material materials with Thermal conductivity of 6.8 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Aluminium | 5.5 - 6.8 % Show Material materials with Aluminium of 5.5 - 6.8 % |
Carbon | 0 - 0.08 % Show Material materials with Carbon of 0 - 0.08 % |
Hydrogen | 0 - 0.02 % Show Material materials with Hydrogen of 0 - 0.02 % |
Iron | 0 - 0.4 % Show Material materials with Iron of 0 - 0.4 % |
Nitrogen | 0 - 0.05 % Show Material materials with Nitrogen of 0 - 0.05 % |
Other | 0 - 0.4 % Show Material materials with Other of 0 - 0.4 % |
Oxygen | 0 - 0.2 % Show Material materials with Oxygen of 0 - 0.2 % |
Titanium | 87.4 - 91 % Show Material materials with Titanium of 87.4 - 91 % |
Vanadium | 3.5 - 4.5 % Show Material materials with Vanadium of 3.5 - 4.5 % |
Yttrium | 0 - 5E-3 % Show Material materials with Yttrium of 0 - 5E-3 % |