ASTM Grade 19 Solution Treated

Want to keep this datasheet? Save it now in your required format

Description

ASTM Grade 19 has very high strength and can be heat treated. It offers good resistance to stress and corrosion.

Equivalent Materials

This material data has been provided by MakeItFrom.com.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueCondition

Density

5.0 g/cm³

Show Material materials with Density of 5.0 g/cm³

Solution Treated

Mechanical

PropertyValueCondition

Elastic modulus

100.0 GPa

Show Material materials with Elastic modulus of 100.0 GPa

Solution Treated

Elongation

17.0 %

Show Material materials with Elongation of 17.0 %

Solution Treated

Tensile strength

910.0 MPa

Show Material materials with Tensile strength of 910.0 MPa

Solution Treated

Yield strength

870.0 MPa

Show Material materials with Yield strength of 870.0 MPa

Solution Treated

Thermal

PropertyValueConditionComment

Coefficient of thermal expansion

9.5e-06 1/K

Show Material materials with Coefficient of thermal expansion of 9.5e-06 1/K

Solution Treated

Melting point

1550.0 - 1815.0 °C

Show Material materials with Melting point of 1550.0 - 1815.0 °C

Typical for Titanium Beta Alloy

Specific heat capacity

520.0 J/(kg·K)

Show Material materials with Specific heat capacity of 520.0 J/(kg·K)

Solution Treated

Thermal conductivity

6.2 W/(m·K)

Show Material materials with Thermal conductivity of 6.2 W/(m·K)

Solution Treated

Chemical properties

PropertyValueCondition

Aluminium

3.0 - 4.0 %

Show Material materials with Aluminium of 3.0 - 4.0 %

Solution Treated

Carbon

0.05 %

Show Material materials with Carbon of 0.05 %

Solution Treated

Chromium

5.5 - 6.5 %

Show Material materials with Chromium of 5.5 - 6.5 %

Solution Treated

Hydrogen

0.02 %

Show Material materials with Hydrogen of 0.02 %

Solution Treated

Iron

0.3 %

Show Material materials with Iron of 0.3 %

Solution Treated

Molybdenum

3.5 - 4.5 %

Show Material materials with Molybdenum of 3.5 - 4.5 %

Solution Treated

Nitrogen

0.03 %

Show Material materials with Nitrogen of 0.03 %

Solution Treated

Other

0.4 %

Show Material materials with Other of 0.4 %

Solution Treated

Oxygen

0.12 %

Show Material materials with Oxygen of 0.12 %

Solution Treated

Titanium

71.1 - 77.0 %

Show Material materials with Titanium of 71.1 - 77.0 %

Solution Treated

Vanadium

7.5 - 8.5 %

Show Material materials with Vanadium of 7.5 - 8.5 %

Solution Treated

Zirconium

3.5 - 4.5 %

Show Material materials with Zirconium of 3.5 - 4.5 %

Solution Treated