General
Property | Value | Temperature |
---|---|---|
Density | 17 g/cm³ Show Material materials with Density of 17 g/cm³ at 23.0 °C | 23.0 °C |
Mechanical
Property | Value | Temperature | Comment |
---|---|---|---|
Elastic modulus | 110 GPa Show Material materials with Elastic modulus of 110 GPa at 23.0 °C | 23.0 °C | |
Elongation | 9.5 % Show Material materials with Elongation of 9.5 % at 23.0 °C | 23.0 °C | |
Poisson's ratio | 0.42 [-] Show Material materials with Poisson's ratio of 0.42 [-] at 23.0 °C | 23.0 °C | Typical for Gold |
Shear modulus | 26 GPa Show Material materials with Shear modulus of 26 GPa at 23.0 °C | 23.0 °C | Typical for Gold |
Tensile strength | 1020 MPa Show Material materials with Tensile strength of 1020 MPa at 23.0 °C | 23.0 °C | |
Yield strength | 830 MPa Show Material materials with Yield strength of 830 MPa at 23.0 °C | 23.0 °C |
Thermal
Property | Value | Temperature | Comment |
---|---|---|---|
Coefficient of thermal expansion | 1.3E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.3E-5 1/K at 23.0 °C | 23.0 °C | |
Melting point | 930 °C Show Material materials with Melting point of 930 °C | ||
Specific heat capacity | 170 J/(kg·K) Show Material materials with Specific heat capacity of 170 J/(kg·K) at 23.0 °C | 23.0 °C | |
Thermal conductivity | 292 - 316 W/(m·K) Show Material materials with Thermal conductivity of 292 - 316 W/(m·K) at 23.0 °C | 23.0 °C | Typical for Gold |
Chemical properties
Property | ||
---|---|---|
Copper | 13.5 - 15.5 % | |
Gold | 70.5 - 72.5 % | |
Other | 0 - 0.4 % | |
Platinum | 8 - 9 % | |
Silver | 4 - 5 % | |
Zinc | 0.7 - 1.3 % |