Density ρ

4.5 g/cm³ at 20 °C

Mechanical

Elastic modulus E

110 GPa at 20 °C

Elongation A

14 % at 20 °C

Tensile strength Rm

710 MPa at 20 °C

Yield strength YS

560 MPa at 20 °C

Thermal

Coefficient of thermal expansion α

9.9E-6 1/K at 20 °C

Specific heat capacity cp

540 J/(kg·K) at 20 °C

Thermal conductivity λ

8.3 W/(m·K) at 20 °C

Chemical properties

Element

Weight %

Comment

Ti

92.4 - 95.4 %

Al

2.5 - 3.5 %

V

2 - 3 %

Ru

0.08 - 0.14 %

C

0 - 0.08 %

More

This material data has been provided by MakeItFrom.com.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.