General
Property | Value | Temperature |
---|---|---|
Density | 4.5 g/cm³ Show Material materials with Density of 4.5 g/cm³ at 23.0 °C | 23.0 °C |
Mechanical
Property | Value | Temperature |
---|---|---|
Elastic modulus | 110 GPa Show Material materials with Elastic modulus of 110 GPa at 23.0 °C | 23.0 °C |
Elongation | 14 % Show Material materials with Elongation of 14 % at 23.0 °C | 23.0 °C |
Tensile strength | 710 MPa Show Material materials with Tensile strength of 710 MPa at 23.0 °C | 23.0 °C |
Yield strength | 560 MPa Show Material materials with Yield strength of 560 MPa at 23.0 °C | 23.0 °C |
Thermal
Property | Value | Temperature | Comment |
---|---|---|---|
Coefficient of thermal expansion | 9.1E-6 1/K Show Material materials with Coefficient of thermal expansion of 9.1E-6 1/K at 23.0 °C | 23.0 °C | |
Melting point | 1668 °C Show Material materials with Melting point of 1668 °C | Typical for Titanium | |
Specific heat capacity | 490 J/(kg·K) Show Material materials with Specific heat capacity of 490 J/(kg·K) at 23.0 °C | 23.0 °C | |
Thermal conductivity | 8.1 W/(m·K) Show Material materials with Thermal conductivity of 8.1 W/(m·K) at 23.0 °C | 23.0 °C |
Chemical properties
Property | ||
---|---|---|
Aluminium | 2.5 - 3.5 % | |
Carbon | 0 - 0.08 % | |
Hydrogen | 0 - 0.02 % | |
Iron | 0 - 0.25 % | |
Nitrogen | 0 - 0.03 % | |
Other | 0 - 0.4 % | |
Oxygen | 0 - 0.15 % | |
Titanium | 92.6 - 95.5 % | |
Vanadium | 2 - 3 % |