General
Property | Temperature | Value |
---|---|---|
Density | 23.0 °C | 8.4 g/cm³ Show Material materials with Density of 8.4 g/cm³ |
Mechanical
Property | Temperature | Value |
---|---|---|
Elastic modulus | 23.0 °C | 210 GPa Show Material materials with Elastic modulus of 210 GPa |
Elongation | 23.0 °C | 14 % Show Material materials with Elongation of 14 % |
Tensile strength | 23.0 °C | 1370 MPa Show Material materials with Tensile strength of 1370 MPa |
Yield strength | 23.0 °C | 950 MPa Show Material materials with Yield strength of 950 MPa |
Thermal
Property | Temperature | Value |
---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.3E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.3E-5 1/K |
Specific heat capacity | 23.0 °C | 470 J/(kg·K) Show Material materials with Specific heat capacity of 470 J/(kg·K) |
Thermal conductivity | 23.0 °C | 13 W/(m·K) Show Material materials with Thermal conductivity of 13 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Carbon | 0 - 0.14 % Show Material materials with Carbon of 0 - 0.14 % |
Chromium | 26 - 30 % Show Material materials with Chromium of 26 - 30 % |
Cobalt | 58.9 - 69 % Show Material materials with Cobalt of 58.9 - 69 % |
Iron | 0 - 0.75 % Show Material materials with Iron of 0 - 0.75 % |
Manganese | 0 - 1 % Show Material materials with Manganese of 0 - 1 % |
Molybdenum | 5 - 7 % Show Material materials with Molybdenum of 5 - 7 % |
Nickel | 0 - 1 % Show Material materials with Nickel of 0 - 1 % |
Nitrogen | 0 - 0.25 % Show Material materials with Nitrogen of 0 - 0.25 % |
Silicon | 0 - 1 % Show Material materials with Silicon of 0 - 1 % |