See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.
Density
ρ10 g/cm³ at 23 °C
Coefficient of thermal expansion
α1.9E-5 1/K at 23 °C
Melting point
Tm780 °C
Specific heat capacity
cp250 J/(kg·K) at 23 °C
Thermal conductivity
λ417 - 428 W/(m·K) at 23 °C
Typical for Silver
Element
Weight %
Comment
89.6 - 91 %
9 - 10.4 %
0 - 5E-3 %
0 - 0.05 %
0 - 0.05 %
This material data has been provided by MakeItFrom.com.