General
Property | Temperature | Value |
---|---|---|
Density | 20.0 °C | 3.1 g/cm³ Show Material materials with Density of 3.1 g/cm³ |
Mechanical
Property | Temperature | Value |
---|---|---|
Elastic modulus | 20.0 °C | 72 GPa Show Material materials with Elastic modulus of 72 GPa |
Elongation | 20.0 °C | 5.5 % Show Material materials with Elongation of 5.5 % |
Elongation A50 | 20.0 °C | 5 - 9 % Show Material materials with Elongation A50 of 5 - 9 % |
Tensile strength | 20.0 °C | 460 - 570 MPa Show Material materials with Tensile strength of 460 - 570 MPa |
Yield strength | 20.0 °C | 470 MPa Show Material materials with Yield strength of 470 MPa |
Yield strength Rp0.2 | 20.0 °C | 370 - 505 MPa Show Material materials with Yield strength Rp0.2 of 370 - 505 MPa |
Thermal
Property | Temperature | Value |
---|---|---|
Coefficient of thermal expansion | 20.0 °C | 2.3E-5 1/K Show Material materials with Coefficient of thermal expansion of 2.3E-5 1/K |
Melting point | 480 °C Show Material materials with Melting point of 480 °C | |
Specific heat capacity | 20.0 °C | 910 J/(kg·K) Show Material materials with Specific heat capacity of 910 J/(kg·K) |
Thermal conductivity | 20.0 °C | 130 W/(m·K) Show Material materials with Thermal conductivity of 130 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Aluminium | 86.9 - 91.4 % Show Material materials with Aluminium of 86.9 - 91.4 % |
Chromium | 0.18 - 0.28 % Show Material materials with Chromium of 0.18 - 0.28 % |
Copper | 1.2 - 2 % Show Material materials with Copper of 1.2 - 2 % |
Iron | 0.5 % Show Material materials with Iron of 0.5 % |
Magnesium | 2.1 - 2.9 % Show Material materials with Magnesium of 2.1 - 2.9 % |
Manganese | 0.3 % Show Material materials with Manganese of 0.3 % |
Other | 0.15 % Show Material materials with Other of 0.15 % |
Silicon | 0.4 % Show Material materials with Silicon of 0.4 % |
Titanium | 0.2 % Show Material materials with Titanium of 0.2 % |
Zinc | 5.1 - 6.1 % Show Material materials with Zinc of 5.1 - 6.1 % |
Zirconium | 0.25 % Show Material materials with Zirconium of 0.25 % |