See where ASTM B541 Age Hardened And Cold Worked falls on the material property chart for Density against Elastic modulus in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.
Density
ρ17 g/cm³ at 20 °C
Coefficient of thermal expansion
α1.3E-5 1/K at 20 °C
Melting point
Tm930 °C
Specific heat capacity
cp170 J/(kg·K) at 20 °C
Electrical conductivity
σel6.96E+7 S/m at 20 °C
Element
Weight %
Comment
70.5 - 72.5 %
13.5 - 15.5 %
8 - 9 %
4 - 5 %
0.7 - 1.3 %