See where ASTM B540 Age Hardened falls on the material property chart for Density against Elastic modulus in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.
Density
ρ13 g/cm³ at 20 °C
Coefficient of thermal expansion
α1.4E-5 1/K at 20 °C
Melting point
Tm1020 °C
Specific heat capacity
cp240 J/(kg·K) at 20 °C
Electrical conductivity
σel3.13E+7 S/m at 20 °C
Element
Weight %
Comment
34 - 36 %
29 - 31 %
13.5 - 14.5 %
9.5 - 10.5 %
9.5 - 10.5 %
This material data has been provided by MakeItFrom.com.