See where ASTM B541 Annealed falls on the material property chart for Density against Elastic modulus in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.
Density
ρ17 g/cm³ at 23 °C
Coefficient of thermal expansion
α1.3E-5 1/K at 23 °C
Melting point
Tm930 °C
Specific heat capacity
cp170 J/(kg·K) at 23 °C
Thermal conductivity
λ292 - 316 W/(m·K) at 23 °C
Typical for Gold
Element
Weight %
Comment
70.5 - 72.5 %
13.5 - 15.5 %
8 - 9 %
4 - 5 %
0.7 - 1.3 %