General
Property | Temperature | Value |
---|---|---|
Density | 23.0 °C | 4.5 g/cm³ Show Material materials with Density of 4.5 g/cm³ |
Mechanical
Property | Temperature | Value |
---|---|---|
Elastic modulus | 23.0 °C | 110 GPa Show Material materials with Elastic modulus of 110 GPa |
Elongation | 23.0 °C | 17 % Show Material materials with Elongation of 17 % |
Tensile strength | 23.0 °C | 710 MPa Show Material materials with Tensile strength of 710 MPa |
Yield strength | 23.0 °C | 560 MPa Show Material materials with Yield strength of 560 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 9.9E-6 1/K Show Material materials with Coefficient of thermal expansion of 9.9E-6 1/K | |
Melting point | 1540 - 1715 °C Show Material materials with Melting point of 1540 - 1715 °C | Typical for Titanium Near Alpha Alloy | |
Specific heat capacity | 23.0 °C | 540 J/(kg·K) Show Material materials with Specific heat capacity of 540 J/(kg·K) | |
Thermal conductivity | 23.0 °C | 8.3 W/(m·K) Show Material materials with Thermal conductivity of 8.3 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Aluminium | 2.5 - 3.5 % Show Material materials with Aluminium of 2.5 - 3.5 % |
Carbon | 0 - 0.08 % Show Material materials with Carbon of 0 - 0.08 % |
Hydrogen | 0 - 0.02 % Show Material materials with Hydrogen of 0 - 0.02 % |
Iron | 0 - 0.25 % Show Material materials with Iron of 0 - 0.25 % |
Nitrogen | 0 - 0.03 % Show Material materials with Nitrogen of 0 - 0.03 % |
Other | 0 - 0.4 % Show Material materials with Other of 0 - 0.4 % |
Oxygen | 0 - 0.15 % Show Material materials with Oxygen of 0 - 0.15 % |
Palladium | 0.04 - 0.08 % Show Material materials with Palladium of 0.04 - 0.08 % |
Titanium | 92.5 - 95.5 % Show Material materials with Titanium of 92.5 - 95.5 % |
Vanadium | 2 - 3 % Show Material materials with Vanadium of 2 - 3 % |