AMS 4928 Grade 5 Annealed

Want to keep this datasheet? Save it now in your required format

Description

This grade is showing excellent strength to weight ratio, higher strength at ambient temperatures than Grades 1 and 2, good creep resistance up to approx 300°C (570 °F), outstanding resistance to corrosion in most natural and many industrial process environments and has approximately half the density of nickel alloys.

Related Standards

Equivalent Materials

This material data has been provided by Alloy Wire International.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

4.42 g/cm³

Show Material materials with Density of 4.42 g/cm³

Mechanical

PropertyTemperatureValue

Elastic modulus

23.0 °C

105 - 120 GPa

Show Material materials with Elastic modulus of 105 - 120 GPa

Tensile strength

23.0 °C

950 - 1100 MPa

Show Material materials with Tensile strength of 950 - 1100 MPa

Thermal

PropertyTemperatureValue

Coefficient of thermal expansion

23.0 °C

9E-6 1/K

Show Material materials with Coefficient of thermal expansion of 9E-6 1/K

Melting point

1605 °C

Show Material materials with Melting point of 1605 °C

Chemical properties

PropertyValue

Aluminium

5.5 - 6.75 %

Show Material materials with Aluminium of 5.5 - 6.75 %

Carbon

0.1 %

Show Material materials with Carbon of 0.1 %

Iron

0.4 %

Show Material materials with Iron of 0.4 %

Nitrogen

0.05 %

Show Material materials with Nitrogen of 0.05 %

Oxygen

0.2 %

Show Material materials with Oxygen of 0.2 %

Vanadium

3.5 - 4.5 %

Show Material materials with Vanadium of 3.5 - 4.5 %

Technological properties

Property
Application areas

Aerospace, Jewellery, Chemical, Springs, Bolts, Fasteners