General
Property | Value | Condition |
---|---|---|
Density | 4.5 g/cm³ Show Material materials with Density of 4.5 g/cm³ | Annealed |
Mechanical
Property | Value | Condition | Shape |
---|---|---|---|
Elastic modulus | 110.0 GPa Show Material materials with Elastic modulus of 110.0 GPa | Annealed | |
Elongation | 17.0 % Show Material materials with Elongation of 17.0 % | Annealed | |
Tensile strength | 620.0 MPa Show Material materials with Tensile strength of 620.0 MPa | Annealed | Sheet, Welded tube, bar |
710.0 MPa Show Material materials with Tensile strength of 710.0 MPa | Annealed | ||
Yield strength | 483.0 MPa Show Material materials with Yield strength of 483.0 MPa | Annealed | Sheet, Welded tube, bar |
560.0 MPa Show Material materials with Yield strength of 560.0 MPa | Annealed |
Thermal
Property | Value | Condition | Comment |
---|---|---|---|
Coefficient of thermal expansion | 9.1e-06 1/K Show Material materials with Coefficient of thermal expansion of 9.1e-06 1/K | Annealed | |
Melting point | 1668.0 °C Show Material materials with Melting point of 1668.0 °C | Typical for Titanium | |
Specific heat capacity | 490.0 J/(kg·K) Show Material materials with Specific heat capacity of 490.0 J/(kg·K) | Annealed | |
Thermal conductivity | 8.1 W/(m·K) Show Material materials with Thermal conductivity of 8.1 W/(m·K) | Annealed |
Chemical properties
Property | Value | Condition | Shape |
---|---|---|---|
Aluminium | 2.5 - 3.5 % Show Material materials with Aluminium of 2.5 - 3.5 % | Annealed | |
2.5 - 3.0 % Show Material materials with Aluminium of 2.5 - 3.0 % | Annealed | Sheet, Welded tube, bar | |
Carbon | 0.08 % Show Material materials with Carbon of 0.08 % | Annealed | Sheet, Welded tube, bar |
Hydrogen | 0.015 % Show Material materials with Hydrogen of 0.015 % | Annealed | |
Iron | 0.25 % Show Material materials with Iron of 0.25 % | Annealed | Sheet, Welded tube, bar |
Nitrogen | 0.03 % Show Material materials with Nitrogen of 0.03 % | Annealed | Sheet, Welded tube, bar |
Other | 0.4 % Show Material materials with Other of 0.4 % | Annealed | |
Oxygen | 0.15 % Show Material materials with Oxygen of 0.15 % | Annealed | Sheet, Welded tube, bar |
Titanium | 92.6 - 95.5 % Show Material materials with Titanium of 92.6 - 95.5 % | Annealed | |
Vanadium | 2.0 - 3.0 % Show Material materials with Vanadium of 2.0 - 3.0 % | Annealed | Sheet, Welded tube, bar |