Density
ρ9 g/cm³ at 23 °C
Coefficient of thermal expansion
α1.5E-5 1/K at 23 °C
Melting point
Tm1170 - 1365 °C
Typical for Nickel Copper Alloy
Specific heat capacity
cp430 J/(kg·K) at 23 °C
Thermal conductivity
λ16 - 45 W/(m·K) at 23 °C
Typical for Nickel Copper Alloy
Element
Weight %
Comment
63 - 72 %
28 - 34 %
0.025 - 0.06 %
0 - 0.3 %
0 - 2.5 %