See where UNS N08020 Annealed falls on the material property chart for Density against Elastic modulus in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.
Density
ρ8.2 g/cm³ at 20 °C
Coefficient of thermal expansion
α1.5E-5 1/K at 20 °C
Specific heat capacity
cp500 J/(kg·K) at 20 °C
Thermal conductivity
λ12 W/(m·K) at 20 °C
Electrical conductivity
σel9.28E+6 S/m at 20 °C
Element
Weight %
Comment
32 - 38 %
29.9 - 44 %
19 - 21 %
3 - 4 %
2 - 3 %
This material data has been provided by MakeItFrom.com.