Nickel 600 Annealed

Want to keep this datasheet? Save it now in your required format

Description

Equivalent Materials

Ashby charts

See where Nickel 600 Annealed falls on the material property chart for Density against Elastic modulus in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

Density

ρ

8.6 g/cm³ at 23 °C

Mechanical

Elastic modulus

E

210 GPa at 23 °C

Show Nickel Chromium Iron Alloy materials with Elastic modulus of 210 GPa at 23 °C

Elongation

A

35 % at 23 °C

Show Nickel Chromium Iron Alloy materials with Elongation of 35 % at 23 °C

Tensile strength

Rm

660 MPa at 23 °C

Show Nickel Chromium Iron Alloy materials with Tensile strength of 660 MPa at 23 °C

Yield strength

YS

280 MPa at 23 °C

Show Nickel Chromium Iron Alloy materials with Yield strength of 280 MPa at 23 °C

Thermal

Coefficient of thermal expansion

α

1.2E-5 1/K at 23 °C

Melting point

Tm

1350 °C

Specific heat capacity

cp

450 J/(kg·K) at 23 °C

Thermal conductivity

λ

14 W/(m·K) at 23 °C

Chemical properties

Element

Weight %

Comment

Ni

72 - 80 %

Cr

14 - 17 %

Fe

6 - 10 %

C

0 - 0.15 %

Cu

0 - 0.5 %

More

This material data has been provided by MakeItFrom.com.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.