Palladium (Pd) Annealed

Want to keep this datasheet? Save it now in your required format

Ashby charts

See where Palladium (Pd) Annealed falls on the material property chart for Density against Elastic modulus in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

Density

ρ

11 g/cm³ at 23 °C

Mechanical

Elastic modulus

E

110 GPa at 23 °C

Show Palladium materials with Elastic modulus of 110 GPa at 23 °C

Elongation

A

12 % at 23 °C

Show Palladium materials with Elongation of 12 % at 23 °C

Poisson's ratio

ν

0.39 [-] at 23 °C

Show Palladium materials with Poisson's ratio of 0.39 [-] at 23 °C

Typical for Palladium

Shear modulus

G

42 GPa at 23 °C

Show Palladium materials with Shear modulus of 42 GPa at 23 °C

Typical for Palladium

Tensile strength

Rm

200 MPa at 23 °C

Show Palladium materials with Tensile strength of 200 MPa at 23 °C

Thermal

Coefficient of thermal expansion

α

1.2E-5 1/K at 23 °C

Melting point

Tm

1550 °C

Specific heat capacity

cp

240 J/(kg·K) at 23 °C

Thermal conductivity

λ

60 - 76 W/(m·K) at 23 °C

Typical for Palladium

Chemical properties

Element

Weight %

Comment

Pd

99.8 - 100 %

Other

0 - 0.2 %

This material data has been provided by MakeItFrom.com.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.