Properties

General

Density

ρ

8.4 g/cm³ at 23 °C

Mechanical

Elastic modulus

E

210 GPa at 23 °C

Show Cobalt Chromium Molybdenum materials with Elastic modulus of 210 GPa at 23 °C

Elongation

A

23 % at 23 °C

Show Cobalt Chromium Molybdenum materials with Elongation of 23 % at 23 °C

Tensile strength

Rm

1030 MPa at 23 °C

Show Cobalt Chromium Molybdenum materials with Tensile strength of 1030 MPa at 23 °C

Yield strength

YS

590 MPa at 23 °C

Show Cobalt Chromium Molybdenum materials with Yield strength of 590 MPa at 23 °C

Thermal

Coefficient of thermal expansion

α

1.3E-5 1/K at 23 °C

Specific heat capacity

cp

470 J/(kg·K) at 23 °C

Thermal conductivity

λ

13 W/(m·K) at 23 °C

Chemical properties

Element

Weight %

Comment

Co

58.9 - 69 %

Cr

26 - 30 %

Mo

5 - 7 %

C

0 - 0.14 %

Fe

0 - 0.75 %

More

This material data has been provided by MakeItFrom.com.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.