See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.
Density
ρ10 g/cm³ at 23 °C
Coefficient of thermal expansion
α2E-5 1/K at 23 °C
Melting point
Tm962 °C
Typical for Silver
Specific heat capacity
cp240 J/(kg·K) at 23 °C
Thermal conductivity
λ417 - 428 W/(m·K) at 23 °C
Typical for Silver
Element
Weight %
Comment
99.9 - 100 %
0 - 0.1 %
This material data has been provided by MakeItFrom.com.