Pewter Type 2 As-Cast

Want to keep this datasheet? Save it now in your required format

Ashby charts

See where Pewter Type 2 As-Cast falls on the material property chart for Density against Elastic modulus in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

Density

ρ

7.3 g/cm³ at 23 °C

Mechanical

Elastic modulus

E

52 GPa at 23 °C

Show Tin materials with Elastic modulus of 52 GPa at 23 °C

Poisson's ratio

ν

0.36 [-] at 23 °C

Show Tin materials with Poisson's ratio of 0.36 [-] at 23 °C

Typical for Tin

Shear modulus

G

18 GPa at 23 °C

Show Tin materials with Shear modulus of 18 GPa at 23 °C

Typical for Tin

Tensile strength

Rm

68 MPa at 23 °C

Show Tin materials with Tensile strength of 68 MPa at 23 °C

Thermal

Coefficient of thermal expansion

α

2.1E-5 1/K at 23 °C

Melting point

Tm

240 °C

Specific heat capacity

cp

220 J/(kg·K) at 23 °C

Thermal conductivity

λ

52 - 74 W/(m·K) at 23 °C

Typical for Tin

Chemical properties

Element

Weight %

Comment

Sn

90 - 93 %

Sb

5 - 7.5 %

Cu

1.5 - 3 %

As

0 - 0.05 %

Fe

0 - 0.02 %

More

This material data has been provided by MakeItFrom.com.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.