General
Property | Temperature | Value |
---|---|---|
Density | 20.0 °C | 7.3 g/cm³ Show Material materials with Density of 7.3 g/cm³ |
Mechanical
Thermal
Property | Temperature | Value |
---|---|---|
Coefficient of thermal expansion | 20.0 °C | 2.1E-5 1/K Show Material materials with Coefficient of thermal expansion of 2.1E-5 1/K |
Melting point | 240 °C Show Material materials with Melting point of 240 °C | |
Specific heat capacity | 20.0 °C | 220 J/(kg·K) Show Material materials with Specific heat capacity of 220 J/(kg·K) |
Chemical properties
Property | Value |
---|---|
Antimony | 5 - 7.5 % Show Material materials with Antimony of 5 - 7.5 % |
Arsenic | 0.05 % Show Material materials with Arsenic of 0.05 % |
Copper | 1.5 - 3 % Show Material materials with Copper of 1.5 - 3 % |
Iron | 0.02 % Show Material materials with Iron of 0.02 % |
Lead | 0.05 % Show Material materials with Lead of 0.05 % |
Tin | 90 - 93 % Show Material materials with Tin of 90 - 93 % |
Zinc | 5E-3 % Show Material materials with Zinc of 5E-3 % |