Density
ρ1.9 g/cm³ at 23 °C
Coefficient of thermal expansion
α2.6E-5 1/K at 23 °C
Melting point
Tm600 °C
Specific heat capacity
cp1040 J/(kg·K) at 23 °C
Thermal conductivity
λ72 W/(m·K) at 23 °C
Element
Weight %
Comment
93.6 - 97.1 %
2.4 - 3.6 %
0.5 - 1.5 %
0.05 - 1 %
0 - 0.04 %