Density
ρ1.9 g/cm³ at 20 °C
Coefficient of thermal expansion
α2.6E-5 1/K at 20 °C
Melting point
Tm470 °C
Specific heat capacity
cp990 J/(kg·K) at 20 °C
Element
Weight %
Comment
88.6 - 91.4 %
8.1 - 9.3 %
0.4 - 1 %
0.13 - 0.35 %
0 - 0.1 %
This material data has been provided by MakeItFrom.com.